Jun 20, 2009 12:13
so I have been doing my own plating of the silver for the dag plates. It has been hit and miss. I just did a great imression, but the next one the iodine didn't take right. I think it is the silver, as I saw the same imperfections in the silver that appeared after the iodine. I think this is still a hygene issue. I need to slow down and wash everything, dry it well etc. I need more space though.
I threw a hissy fit yesterday due to tripping over everything and a lot of things got cleaned up, but I still don't have the room I need. The issue is I need about 10 linear feet to have everything in a production line. Sadly I only have about 3 feet at a time, and that is just a little too little to do any of the steps well. Looks like I need to throw another fit.